MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Cotronics Resbond™ 954 High Temperature Ceramic Adhesive, Stainless Steel Composition
Categories: Ceramic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 17.2 MPa2500 psi
Compressive Strength 31.0 MPa4500 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
10.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.44 W/m-K10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1090 °C2000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 304SS Washers and Studs
Overview of materials for AISI 4000 Series Steel
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 310 SS Washers and Studs
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 330 SS Washers and Studs
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems Inconel 601 Washers and Studs

CCOTR0160 / 767

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.