MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Rogers Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
  • Side 1: Uncured Silicone Rubber
  • Substrate: Style 7628 Fiberglass
  • Side 2: Uncured Silicone Rubber
  • Interleave: 2.5 mil Polyethylene

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 203 microns8.00 milSubstrate; Arlon SQA-TMS-003
 229 microns9.00 milSide 1; Arlon SQA-TMS-003
 508 microns20.0 milSide 2; Arlon SQA-TMS-003
 940 microns37.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Silicone Property; ASTM D2240
Tensile Strength 5.52 MPa800 psiSilicone Property; ASTM D412
Elongation at Break 225 %225 %Silicone Property; ASTM D412
Tear Strength 15.8 kN/m90.0 pliSilicone Property; ASTM D624
Peel Strength 1.51 kN/m8.60 pliBond Strength (S1 to S2); Arlon SQA-TMS-011
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 27.2 kV/mm690 kV/inArlon SQA-TMS-020
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
UL RTI, Electrical 220 °C428 °FFile E54153
UL RTI, Mechanical without Impact 220 °C428 °FFile E54153
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Post Cure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 21.1 °C
6.00 Month
@Temperature 70.0 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 51276R020 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51276R015 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate

PARL9768 / 148921

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.