MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupox® GP2306FY PBT+GF30%
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Injection Molding, PBT+GF30%Flame Retardant, GWIT

Application: IT/OA, E&E (Connector)

CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.66 g/cc1.66 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0030 - 0.010 cm/cm
@Thickness 3.20 mm
0.0030 - 0.010 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 108 MPa
@Thickness 3.20 mm
15700 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 4.0 %
@Thickness 3.20 mm
>= 4.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 157 MPa
@Thickness 3.20 mm
22800 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 9.81 GPa
@Thickness 3.20 mm
1420 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 0.686 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.29 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Dielectric Strength 28.0 kV/mm711 kV/inASTM D149
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 250 V250 VSolution A; IEC 60112
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=0.710 mm
7.0 - 15 sec
@Thickness >=0.0280 in
 30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 0.710 mm
60 - 120 arcs
@Thickness 0.0280 in
 60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F@ Break; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
@Thickness 6.40 mm
419 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
@Thickness 6.40 mm
401 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  140 °C
@Thickness >=0.710 mm
284 °F
@Thickness >=0.0280 in
 140 °C
@Thickness >=1.50 mm
284 °F
@Thickness >=0.0591 in
 140 °C
@Thickness >=3.00 mm
284 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  140 °C
@Thickness >=0.710 mm
284 °F
@Thickness >=0.0280 in
 140 °C
@Thickness >=1.50 mm
284 °F
@Thickness >=0.0591 in
 140 °C
@Thickness >=3.00 mm
284 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  140 °C
@Thickness >=0.710 mm
284 °F
@Thickness >=0.0280 in
 140 °C
@Thickness >=1.50 mm
284 °F
@Thickness >=0.0591 in
 140 °C
@Thickness >=3.00 mm
284 °F
@Thickness >=0.118 in
Flammability, UL94  V-0
@Thickness >=0.710 mm
V-0
@Thickness >=0.0280 in
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 235 - 250 °C455 - 482 °FInjection Molding
Middle Barrel Temperature 235 - 250 °C455 - 482 °FInjection Molding
Front Barrel Temperature 240 - 250 °C464 - 482 °FInjection Molding
Nozzle Temperature 245 - 255 °C473 - 491 °FInjection Molding
Melt Temperature 245 - 255 °C473 - 491 °FInjection Molding
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection Molding
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyimide, Unfilled
Envalior Arnite® B427 SE/R PBT-GF35 FR(17)
Envalior Arnite® B436 SE PBT-GF30 FR(17)
Aclo Accucomp PET PET008L
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT

PLAY344 / 148354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.