MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODUR® TD6400 + BAYTEC® XL TMP-TIPA + PLASTICIZER V10 (Catalyst SD6-40), 40 A Polyurethane, TDI- Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccPLASTICIZER V10
 1.05 g/cc1.05 g/ccBAYTEC® XL TMP-TIPA
 1.19 g/cc1.19 g/ccDESMODUR® TD6400
 1.23 g/cc1.23 g/cc
Viscosity 15 cP15 cPPLASTICIZER V10
 75 cP75 cPBAYTEC® XL TMP-TIPA
 2000 cP2000 cPDESMODUR® TD6400
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040DIN 53505
 40
@Temperature 80.0 °C
40
@Temperature 176 °F
DIN 53505
 48
@Temperature -5.00 °C
48
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 15.0 MPa2180 psiDIN 53504
Tensile Stress at Strain 0.200 MPa
@Strain 10 %
29.0 psi
@Strain 10 %
DIN 53504
Elongation at Break 430 %430 %DIN 53504
100% Modulus 1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
DIN 53504
200% Modulus 1.70 MPa
@Strain 200 %
247 psi
@Strain 200 %
DIN 53504
300% Modulus 2.80 MPa
@Strain 300 %
406 psi
@Strain 300 %
DIN 53504
Resilience 2525[%]; DIN 53512
Tear Strength 6.00 kN/m34.2 pliwith nick; ISO 34-1
 22.0 kN/m126 pliwithout nick; ISO 34-1
Abrasion 200200[mm3]; ISO 4649
Compression Set 5.0 %
@Temperature 70.0 °C,
Time 79200 sec
5.0 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FPLASTICIZER V10
 80.0 °C176 °FDESMODUR® TD6400
 90.0 °C194 °FBAYTEC® XL TMP-TIPA
Mold Temperature 110 °C230 °F
Pot Life 18.0 min18.0 min
 
Descriptive Properties
AppearanceliquidPLASTICIZER V10
 solidDESMODUR® TD6400
 solidBAYTEC® XL TMP-TIPA
Content0.35Catalyst SD6-40 % / total (by weight) (catalyst at the head)
 100Parts by weight of prepolymer
 28Parts by weight of PLASTICIZER V10
 4.05-4.45%NCO
 4.6Parts by weight of BAYTEC® XL TMP-TIPA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mearthane Durethane™ S DS-340A Solid Polyurethane Elastomer
Mearthane Durethane™ S DS-240A Solid Polyurethane Elastomer
Mearthane Durethane™ C 30-55A Polyurethane
Dow BETAMATE™ 7200 Polyurethane Prepolymer
Covestro DESMODUR® TD6400 + BAYTEC® XL TMP + PLASTICIZER V10 (Catalyst SD6-40), 40 A Polyurethane, TDI- Ester

PCOVEST0600 / 202383

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.