MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton 801 Industrial & Marine Solvent
Categories: Fluid; Solvent

Material Notes: Description: Chesterton® 801 Industrial & Marine Solvent is an industrial strength, multiple purpose, water based degreaser. It is an easy to use product that can be applied with sprayers, foamers, steam cleaners, sponge, mop or brush. Applications for 801 Industrial & Marine Solvent (IMS) can be found almost everywhere. It removes cooling and cutting oils prior to inspection, assembly, and shipping. 801 IMS neatly cleans tanks, engines, motors, tools and working areas. It does an excellent job flushing coolant systems. When used in marine applications, it efficiently removes rot, mildew and other fungi from hulls. An ideal bilge cleaner, it emulsifies and combines with oil, grease, gasoline, chemicals, sludge and fuel to lift and remove them from surfaces. 801 IMS is NSF registered for use in federally inspected meat and poultry plants, It can be used to clean food processing equipment, bottling machines and wax and grease from vents, stoves, hoods and ovens. Chesterton 801 Industrial & Marine Solvent is truly a versatile and economical multi-surface cleaner and degreaser.

Features:

  • Nonflammable
  • Wide Dilution Range
  • Economical, Efficient
  • Multi-Service
  • Biodegradable
  • Stable, Clinging Foam
  • NSF A1, A4, A8 – Registration number 133965

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
pH 1313
 
Descriptive Properties
AppearanceRed, Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 801 TFE 20 Acetal (POM), Glass Fiber - PTFE Lubricated
Karina 801-18/489-C-IS Gray PVC Compound
Karina 801-10/88-CR White PVC Compound
Glyptal 2600 Alkyd Nitrocellulose Lacquer
Glyptal 1559 Alkyd Nitrocellulose Lacquer

PPTCHS053 / 138165

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.