MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Akulon® F-X9182 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Low/Medium Viscosity

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³dry; ISO 1183
Viscosity  150000 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
150000 cP
@Shear Rate 1000 1/s,
Temperature 554 °F
 175000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
175000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
 175000 cP
@Shear Rate 0.1 1/s,
Temperature 290 °C
175000 cP
@Shear Rate 0.1 1/s,
Temperature 554 °F
 200000 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
200000 cP
@Shear Rate 1000 1/s,
Temperature 446 °F
 225000 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
225000 cP
@Shear Rate 0.1 1/s,
Temperature 500 °F
 350000 cP
@Shear Rate 0.1 1/s,
Temperature 230 °C
350000 cP
@Shear Rate 0.1 1/s,
Temperature 446 °F
Viscosity Measurement 2.62.6RSV formic acid, 1g/100ml; DSM method
Viscosity Number 160 cm³/g1.60 dl/gISO 307, 1157, 1628
Thickness 50.0 microns1.97 milfilm
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°Fdry; ISO 11359-1/-2
 
Descriptive Properties
Extrusion TypeCast Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shakespeare Resistat® F9222 B040 Nylon 6 Monofilament
NYCOA 870 PA 6
Nurel Engineering Polymers Promyde® B26 C PA 6
Envalior Akulon® F-X9215 PA6
Envalior Akulon® F-X9183 PA6

PDSM9754 / 161375

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.