MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

China Tungsten YG640 Tungsten Carbide
Categories: Ceramic; Carbide

Material Notes: Good thermal strength, high resistance to wear, impact and oxidation. Continuous or intermittent cutting of heavy work pieces of cast irons, milling and planning of refractory steel with high strength.

Information provided by China Tungsten

Key Words: ISO K30~K40/M40
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 13.2 g/cc0.477 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 9191
Flexural Strength 2410 MPa350000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
China Tungsten ZK40 Tungsten Carbide
H.C. Starck Amperit® 516.074 Tungsten Carbide - Cobalt (WC-Co) 88-12
PSM Industries PolyAlloys MIM-WC-9Co Tungsten Carbide
Tungsten Carbide, WC
H.C. Starck Amperit® 515.074 Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12

NCHIN053 / 78895

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.