MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.

Data Provided by the manufacturer, Coors Ceramics Co.

Key Words: Al2O3; aluminum oxide, alumina
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.60 g/cc0.130 lb/in³ASTM C20
Water Absorption 0.00 %0.00 %ASTM C373
Particle Size 4.0 µm4.0 µmAverage Crystal Size - Thin Section Test
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 10.410.41000 g load
Hardness, Rockwell 45 N 7575GPa
Tensile Strength, Ultimate 221 MPa32100 psiACMA Test #4
Modulus of Elasticity 276 GPa40000 ksiASTM C848
Flexural Strength 338 MPa49000 psiASTM F417
Compressive Strength 2482 MPa360000 psiASTM C773
Poissons Ratio 0.220.22ASTM C848
Fracture Toughness 3.00 - 4.00 MPa-m½2.73 - 3.64 ksi-in½Notched Beam
Shear Modulus 113 GPa16400 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D1829
 500000 ohm-cm
@Temperature 1000 °C
500000 ohm-cm
@Temperature 1830 °F
ASTM D1829
 4.00e+8 ohm-cm
@Temperature 500 °C
4.00e+8 ohm-cm
@Temperature 932 °F
ASTM D1829
Dielectric Constant 8.8
@Frequency 1e+6 Hz
8.8
@Frequency 1e+6 Hz
Dielectric Strength 8.30 kV/mm211 kV/inac; ASTM D116
Dielectric Loss Index 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
ASTM D2520
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.10 µm/m-°C
@Temperature 25.0 - 1000 °C
4.50 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.920 J/g-°C0.220 BTU/lb-°FASTM E1269
Thermal Conductivity 16.7 W/m-K116 BTU-in/hr-ft²-°FASTM C408
Maximum Service Temperature, Air 1500 °C2730 °FNo Load
 
Component Elements PropertiesMetricEnglishComments
Al2O3 90 %90 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trimay® Wear Plate T156 Iron-based Steel Overlay
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
CeramTec 771 94% Alumina (Al2O3)
CeramTec 848 Zirconia, ZrO2•MgO
CeramTec B 601 Alumina, 98.5%

CA7B / 377

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.