MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 105 CC SI 2  Polypropylene (PP) Glass Fiber 30% - Chemically Coupled - Silicone 2%  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Glass Fiber 30% - Chemically Coupled - Silicone 2%

Comments:

  • Glass Fiber
  • Chemically Coupled
  • Silicone Lubricated

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Filler Content 30 %30 %
Water Absorption 0.040 %0.040 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage  0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 0.0050 cm/cm
@Thickness 6.35 mm
0.0050 in/in
@Thickness 0.250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Tensile Strength, Ultimate 82.7 MPa12000 psiASTM D638
Elongation at Break >= 2.5 %>= 2.5 %ASTM D638
Modulus of Elasticity 6.89 GPa1000 ksiASTM D638
Flexural Yield Strength 117 MPa17000 psiASTM D790
Flexural Modulus 4.83 GPa700 ksiASTM D790
Compressive Yield Strength 82.7 MPa12000 psiASTM D695
Izod Impact, Notched 1.01 J/cm
@Thickness 3.17 mm
1.90 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inS/T; ASTM D149
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
Dry; ASTM D150
Arc Resistance 125 sec125 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
@Temperature 20.0 °C
20.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.331 W/m-K2.30 BTU-in/hr-ft²-°FThrough-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 157 °C315 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
Per testing by RTP Company; ASTM D635
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 227 °C380 - 440 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Overview of materials for 1000 Series Aluminum
RTP Company RTP 140 HF Z  Polypropylene (PP) Calcium Carbonate 40% - High Flow - FDA Type
RTP Company RTP 105 HI  Polypropylene (PP) Glass Fiber 30% - High Impact

PR3058 / 62320

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.