MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) BLUESIL™ V-1062 Hi-Pro Blue Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL™ V-1062 is a high strength, two-component, tin catalyzed, room temperature cure silicone rubber. It is designed as a 14 Durometer (Shore A), very pourable rubber providing excellent physical properties, long library life, and excellent detail reproduction. BLUESIL™ V-1062 can also be used in vacuum demolding.

Applications:

  • Figurine and giftware casting using Polyester, Polyurethane, Plaster or Gypsum
  • Glove molds-one piece and suitcase styles
  • Transfer print pads

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/cc
Viscosity 32000 cP32000 cPMixed
 50000 cP50000 cPPart A, Base Component
Storage Temperature 24.0 °C75.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1212ASTM D2240
 151524 hr thick section
Tensile Strength 2.59 MPa375 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
Tear Strength 19.3 kN/m110 pliASTM D624, Die B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
50% RH
Pot Life 90.0 min90.0 min
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
ColorBluePart B, Catalyst Component
 WhitePart A, Base Component
Work Life8 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Coastal Enterprises Plus™ PBLT-60 High Density Urethane Foam
Renishaw Vacusil 200 Liquid Silicone Rubber
Renishaw 5175 Polyurethane Resin
Coastal Enterprises Plus™ PBLT-48 High Density Urethane Foam
BCC Products Kwik Kast BC 8002 Urethane Casting

PBLUST053 / 191029

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.