MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® DP 2131/20 H2.0 900051 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: PA 6, 20% glass fibers, injection molding, heat-aging stabilized, improved surface finish, improved resistance to weathering

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0035 cm/cm0.0035 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0054 cm/cm0.0054 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 2.00e+13 ohm2.00e+13 ohmIEC 60093
Dielectric Constant  4.27
@Frequency 1e+6 Hz
4.27
@Frequency 1e+6 Hz
IEC 60250
 9.34
@Frequency 100 Hz
9.34
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.065
@Frequency 1e+6 Hz
0.065
@Frequency 1e+6 Hz
IEC 60250
 0.22
@Frequency 100 Hz
0.22
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °Finjection molding
 270 - 290 °C518 - 554 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 120 °C176 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Domo TECHNYL® 2417IG PA66, 20% glass fiber, DRY
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Domo TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, Conditioned

PLANW9473 / 208324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.