MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nylene® NX3411 Nylon 6
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Film Grade. Nylene NX3411 is an extrusion grade nylon 6 resin suitable for film co-extrusion applications and blown film. It has excellent melt stability and good melt strength. Nylene NX3411 has superior grease resistance, toughness, resistance to abrasion, and does not absorb food odors. Nylene NX3411 meets the requirements of FDA regulation 21 CFR 177.1500 for direct food contact.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 38.0 MPa5510 psiOrientation not specified; ASTM D882
Film Elongation at Break, MD 290 %290 %Orientation not specified; ASTM D882
Secant Modulus 0.650 GPa94.3 ksiASTM D882
Elmendorf Tear Strength MD 56 g56 gOrientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 60.0 MPa8700 psiOrientation not specified; ASTM D882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nylene® NX3055I Nylon 6
Nylene® 615SA Nylon 6, Film Grade
Nylene® 615I Nylon 6, Film Grade
Nylene® 615 Nylon 6, Film Grade

PN6C45 / 54203

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.