MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Johnson Matthey SW 850 Platinum w/ 15% Iridium Jewelry Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Material Notes: Springs, watch backs. Copper, cobalt, gold, iridium, palladium and ruthenium alloy easily with platinum. The differences between the alloys reflect the hardening of the alloying element itself.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 21.5 g/cc0.777 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160160Annealed
Elongation at Break 15 %15 %Annealed
 
Thermal PropertiesMetricEnglishComments
Melting Point 1800 - 1820 °C3270 - 3310 °F
Solidus 1800 °C3270 °F
Liquidus 1820 °C3310 °F
 
Component Elements PropertiesMetricEnglishComments
Iridium, Ir 15 %15 %
Platinum, Pt 85 %85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey SC 850 Platinum w/ 15% Palladium Jewelry Alloy
Johnson Matthey HM Platinum w/ 5% Ruthenium Jewelry Alloy
Goodfellow Platinum 90/Iridium 10 Alloy
Johnson Matthey HS Platinum Jewelry Alloy
Johnson Matthey SC 900 Platinum w/ 10% Palladium Jewelry Alloy

NJMMJ66 / 97758

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.