MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M SJ6561 Protective Product, Molded Shapes
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 3M Bumpon Protective Products Quite Clear SJ6500 Series are molded cushioning products that utilize a special, soft polyurethane formulation and synthetic rubber adhesive system. This unique construction provides an excellent cushioning stop, spacer or non-skid foot solution, with enhance sound damping characteristics. The 3M high tack, pressure-sensitive adhesive system is protected with a polyester liner, making individual Bumpon removal and application quick and easy.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore M 5656ASTM D2240
Tensile Strength at Break 1.86 MPa270 psiASTM D412
Elongation at Break 170 %170 %ASTM D412
Coefficient of Friction, Dynamic 1.81.8Formica laminate; ASTM D1894
 2.32.3Wood; ASTM D1894
 2.82.8Stainless Steel; ASTM D1894
 2.82.8Glass; ASTM D1894
Taber Abrasion, mg/1000 Cycles 0.0300.030H18, 1 kg; ASTM C501
 
Descriptive Properties
Adhesive TypeR-25 Synthetic Rubber
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Lo-Skid® LS7000/LS7100 Series High Density Bumper and Footpad Urethane Foam
3M SJ6553 Protective Product, Molded Shapes
3M SJ6512 Protective Product, Molded Shapes
3M SJ6506 Protective Product, Molded Shapes
3M Bumpon™ SJ5832 Resilient Rollstock

PMM35259 / 170006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.