MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccISO 1183
Filler Content 30 %30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa
@Temperature 23.0 °C
12300 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 1.6 %
@Temperature 23.0 °C
1.6 %
@Temperature 73.4 °F
ISO 527-2
Tensile Modulus 9.00 GPa
@Temperature 23.0 °C
1310 ksi
@Temperature 73.4 °F
ISO 527-2
Charpy Impact Unnotched 3.40 J/cm²
@Temperature 23.0 °C
16.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 224 °C435 °F
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
Glow Wire Flammability Index 960 °C1760 °FIEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 270 °C446 - 518 °F
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 110 - 130 °C230 - 266 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Descriptive Properties
AdditiveUV Stabilizer
FeaturesFlame Retardant
 Halogen Free
FormsPellets
Generic MaterialPBT
Generic NamePolybutylene Terephthalate (PBT)
Regional AvailabilityEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT)
Avient Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT)
Avient Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT)
Avient Edgetek® PS-20GF/000 NATURAL Polybutylene Terephthalate (PBT)
Avient Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)

PH0POL1323 / 145892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.