MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Acetic acid vapors are released from the sealant surface as a by-product of cure.

RTV102, RTV103, RTV108, and RTV109 sealants are standard strength paste consistency products which can be applied to vertical and overhead surfaces where pourable/self-leveling sealants are not practical.

Key Performance Properties:

  • One-component products
  • Capability to cure at room temperature and ambient humidity
  • Self adhesion properties
  • Low temperature flexibility
  • High temperature performance
  • Excellent weatherability and ozone and chemical resistance
  • Excellent electrical insulation properties

Applications:

General purpose bonding, sealing, electrical insulation, formed-in-place gaskets. Can be applied to vertical or overhead surfaces.

FDA 21 CFR 177.2600 USDA NSF International Std. No. 51

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030
Tensile Strength, Ultimate 2.75 MPa398 psi
Elongation at Break 450 %450 %
Adhesive Bond Strength 1.37 MPa199 psiAt 100% cohesive failure
Tear Strength 7.85 kN/m44.8 pli
Peel Strength 7.01 kN/m40.0 pliAt 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+15 ohm-cm3.00e+15 ohm-cm
Dielectric Constant 2.8
@Frequency 60 Hz
2.8
@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm508 kV/in
Dissipation Factor 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
150 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.209 W/m-K1.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °FContinuous
 260 °C500 °FIntermittent
Brittleness Temperature -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 20.0 min0.333 hour
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USDA YesYes
 
Descriptive Properties
Application rate400 g/min
ColorBlack
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red
Overview of materials for Silicone Rubber
Overview of materials for Liquid Silicone Rubber
Momentive Performance Materials TSE 221-3U Heat Cured Rubber

PGESIL008 / 40999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.