MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell AF/Armaflex® Insulation
Categories: Other Engineering Material

Material Notes: Description: Highly-flexible, closed-cell insulation material with high water vapor diffusion resistance and low thermal conductivity.

Special Features: Increasing insulation wall thicknesses for tubes ensures that the surface temperature is maintained as the pipe diameter is increased.

Application: Thermal insulation/protection of pipes, vessels and ducts (incl. elbows, fittings, flanges etc.) in industrial and process equipment facilities.

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Absorption Coefficient <= 0.45<= 0.45EN ISO 354
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity <= 0.0330 W/m-K<= 0.229 BTU-in/hr-ft²-°FTubes (AF-1 to AF-4); EN ISO 13787
 <= 0.0330 W/m-K<= 0.229 BTU-in/hr-ft²-°FSheets (AF-13MM to AF32MM); EN ISO 13787
 <= 0.0360 W/m-K<= 0.250 BTU-in/hr-ft²-°FSheets (AF-50MM; EN ISO 13787
 <= 0.0360 W/m-K<= 0.250 BTU-in/hr-ft²-°FTubes (AF-5 to AF-6); EN ISO 13787
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell AP Armaflex® FS 1 1/2" & 2" Duct Liner
Armacell AC/Accoflex® Tube Insulation
Armacell AP/Armaflex® Black LapSeal™ Tube Insulation with Reinforced Lap Seal

PARMD169 / 186780

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.