Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross than SAC305 and other Sn/Cu based alloys Features - Shiny, smooth solder joints similar to Sn/Pb solder
- Low cost - does not contain Ag
- Lower dross formation than other SAC and Sn/Cu-based alloys
- Less copper erosion than SAC305
- Compatible with other Sn/Cu-based alloys - no need to dump the pot
- Available in a solder bar for wave soldering and cored wire for rework applications