MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical SEETEC EF443 Ethylene Vinyl Acetate  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Characteristics: Good Mechanical Properties and Good Optical Properties

Applications: Agricultural Film

CSA No. 24937-78-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.928 - 0.932 g/cc0.928 - 0.932 g/ccASTM D1505
Melt Flow 0.80 - 1.2 g/10 min
@Load 2.61 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min
@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 19.6 MPa2840 psi500mm/min; ASTM D638
Film Elongation at Break, MD 400 %400 %500 mm/min; ASTM D638
Film Elongation at Break, TD 650 %650 %500 mm/min; ASTM D638
Elongation at Break 650 %650 %500 mm/min; ASTM D638
2% Secant Modulus 0.650 GPa94.3 ksi500mm/min; ASTM D638
Elmendorf Tear Strength MD 220 g220 gASTM D1922
Elmendorf Tear Strength TD 260 g260 gASTM D1922
Dart Drop Test >= 400 g>= 0.882 lbASTM D1709
Film Tensile Strength at Break, MD 30.4 MPa4410 psi500mm/min, Ultimate; ASTM D638
Film Tensile Strength at Break, TD 30.4 MPa4410 psi500mm/min, Ultimate; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 94.0 °C201 °F10°C/min; ASTM D3418
Vicat Softening Point 85.0 °C185 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 3.5 %3.5 %ASTM D1003
Gloss 105 %105 %45°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 150 Ethylene Vinyl Acetate
Dow Elvax® 760 Ethylene Vinyl Acetate
Armacell OleTex® BCJN 200 EVA/LDPE Foam
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate
Dow Elvax® 470 Ethylene Vinyl Acetate

PLAY228 / 148238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.