MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Bayflex® 956 Polyether-based Polyurethane System, Density 34 pcf
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Bayflex 956 is a fully compounded, water-blown, polyether-based polyurethane system consisting of two liquid components..

Properties / Applications: Bayflex 956 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown. Component A is a modified diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. The Bayflex 956 system is used in the manufacture of microcellular polyurethane shoe soles. Soles prepared from these components combine light weight, comfort, and durability. Processibility and dynamic flexural properties are excellent over a wide range of densities. The combination of excellent physical properties and ease of processing has made the Bayflex 956 system a prime soling material for fashion and casual shoes. As with any product, use of the Bayflex 956 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.480 - 0.540 g/cc0.480 - 0.540 g/ccMolded
 1.06 g/cc1.06 g/ccPolyol (Component B)
 1.20 g/cc1.20 g/ccIsocyanate (Component A)
Viscosity 1100 cP1100 cPIsocyanate (Component A)
 1000 - 1500 cP1000 - 1500 cPPolyol (Component B)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 51 - 5851 - 58ASTM D2240
Tensile Strength at Break 3.45 - 4.14 MPa500 - 600 psiASTM D412
Elongation at Break 350 - 450 %350 - 450 %ASTM D412
Tear Strength 3.33 - 4.38 kN/m19.0 - 25.0 pliBlack
 15.8 - 19.3 kN/m90.0 - 110 pliDie C; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
Flash Point 126 °C259 °FPolyol (Component B)
 207 °C405 °FIsocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 43.0 - 51.0 °C109 - 124 °F
Moisture Content 0.38 - 0.44 %0.38 - 0.44 %Polyol (Component B)
 
Descriptive Properties
Content18.7-19.1%NCO, Isocyanate (Component A)
Hydroxyl number[mg KOH/g], Polyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayflex® 962 Polyether-based Polyurethane System, Density 34 pcf
Armacell Monarch® F-03944 (Dark Gray) Pure EPDM Foam
Covestro Bayflex® 970 Polyether-based Polyurethane System, Density 34 pcf
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU
Covestro Bayflex® 906 Polyether-based Polyurethane System, Density 29 pcf

PCOVEST0130 / 201913

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.