MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reade Advanced Materials Ferritan C Steel/Titanium Carbide Composite
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite

Material Notes: A machinable and hardenable alloy/steel bonded titanium carbide. The ultra-hard, rounded titanium carbide grains are uniformly distributed throughout a hardenable steel alloy matrix. Fabrication in the annealed state is accomplished with ordinary tools and equipment, followed by conventional heat treatment to obtain maximum hardness. Used for high-production tooling, highly wear resistant parts, resistance to environmental attack, high temperatures and severe corrosion, and for additional toughness.

Information provided by Reade Advanced Materials.

Key Words: TiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.60 g/cc0.238 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 44 - 4644 - 46Annealed
 68 - 7068 - 70Heat Treated
 
Descriptive Properties
TiC Content (vol%)45

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cunico® Hard Magnetic Alloy
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel
Neodymium® 30H Hard Magnetic Alloy
Schwarzkopf Plansee PM 2000, Sheet Grain Class 6 ODS Iron Alloy Sheet
Aluminum - SiC Metal Matrix Composite

NREADE026 / 199548

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.