MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott Transparent ITO Conducting Oxide Coating
Categories: Ceramic; Oxide

Material Notes: Spectral range 400-5000 nm

A transparent conducting coating (TCO) ensures both electrical conductivity and optically transparency.

Information provided by SCHOTT.

Key Words: Indium Tin Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 6.0 - 14 ohm6.0 - 14 ohm
 90 - 110 ohm90 - 110 ohm
 270 - 330 ohm270 - 330 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) <= 0.010
@Wavelength 450 - 650 nm
<= 0.010
@Wavelength 450 - 650 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
SunChemical Gwent F2071018D1 Transparent ITO Coated Film
Indium Corp. Fine ITO Indium Tin Oxide
Indium Corp. Standard ITO Indium Tin Oxide
Tin, Sn

CSGT9833 / 183086

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.