MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akroloy® PA GF 30 natural (3177) PA 66 + PA 6I/6T Dry, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Akroloy PA GF 30 natural (3177) is a 30% glass fiber reinforced polyamide blend with high stiffness and strength, even in conditioned state. Applications are components with high dimensional stability, independent from moisture content. Akroloy PA GF 30 is an alternative for aluminum and zinc diecast alloys.

Features:

  • Good Dimensional Stability
  • High Stiffness
  • High Strength
Uses: Metal Replacement

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Filler Content 30 %30 %ISO 1172
Moisture Absorption 1.55 %
@Temperature 70.0 °C
1.55 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 4.5 - 5.0 %4.5 - 5.0 %ISO 62
Linear Mold Shrinkage, Flow <= 0.0010 cm/cm<= 0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
Spiral Flow 75.7 cm29.8 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 240 MPa34800 psiH 961/30; ISO 2039-1
Tensile Strength at Break 210 MPa30500 psi5 [mm/min]; ISO 527-2
 105 MPa
@Treatment Temp. 140 - 150 °C,
Time 1.80e+7 sec
15200 psi
@Treatment Temp. 284 - 302 °F,
Time 5000 hour
50% Loss of Tensile Strength; IEC 60216
 105 MPa
@Treatment Temp. 140 - 150 °C,
Time 7.20e+7 sec
15200 psi
@Treatment Temp. 284 - 302 °F,
Time 20000 hour
50% Loss of Tensile Strength; IEC 60216
Elongation at Break 3.0 %3.0 %5 [mm/min]; ISO 527-2
Tensile Modulus 10.5 GPa1520 ksi1 [mm/min]; ISO 527-2
Flexural Strength 265 MPa38400 psi2 mm/min; ISO 178
Flexural Modulus 9.30 GPa1350 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Melting Point 255 °C491 °FDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75-2/A
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 100P BK602 POM
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
Akro-Plastic Akromid® A 28 GF 30 1 GIT (4619) PA 66 Conditioned, 30% Glass Filled
Akro-Plastic Akromid® A 28 GF 30 1 GIT (4619) PA 66 Dry, 30% Glass Filled

PAKRO101 / 182688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.