MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

10% Glass Reinforced.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: Poly(Acrylonitrile Butadiene Styrene); ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 97.0 MPa14100 psiASTM D790
Flexural Modulus 3.90 GPa566 ksiASTM D790
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256
Izod Impact, Unnotched 2.46 J/cm4.61 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 235 - 266 °C455 - 511 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

PASH4G / 24923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.