MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics REFCAST C High Alumina Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Manufacturer produces a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industries such as steel, cement, petrochemical and non-ferrous industries.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 2.10 g/cc>= 0.0759 lb/in³Dried at 110°C
Grain Size <= 5000 µm<= 5000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.00294 GPa
@Temperature 1100 °C
0.426 ksi
@Temperature 2010 °F
 0.00637 GPa
@Temperature 110 °C
0.924 ksi
@Temperature 230 °F
 0.00834 GPa
@Temperature 1500 °C
1.21 ksi
@Temperature 2730 °F
Compressive Strength  24.5 MPa
@Temperature 1100 °C
3560 psi
@Temperature 2010 °F
Cold Crushing
 37.3 MPa
@Temperature 110 °C
5400 psi
@Temperature 230 °F
Cold Crushing
 49.0 MPa
@Temperature 1500 °C
7110 psi
@Temperature 2730 °F
Cold Crushing
 19.6 MPa
@Time 86400 sec
2840 psi
@Time 24.0 hour
Cold Crushing
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.872 W/m-K
@Temperature 400 °C,
Time 10800 sec
6.05 BTU-in/hr-ft²-°F
@Temperature 752 °F,
Time 3.00 hour
 0.988 W/m-K
@Temperature 800 °C,
Time 10800 sec
6.86 BTU-in/hr-ft²-°F
@Temperature 1470 °F,
Time 3.00 hour
 0.988 W/m-K
@Temperature 600 °C,
Time 10800 sec
6.86 BTU-in/hr-ft²-°F
@Temperature 1110 °F,
Time 3.00 hour
Maximum Service Temperature, Air 1500 °C2730 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 50 %>= 50 %
Fe2O3 <= 1.5 %<= 1.5 %
 
Descriptive Properties
Permanent Linear Change<-0.06800°C
 <-0.121100°C
 <-0.851500°C
Refractoriness1650°C
Thermal Expansion0.55Reversible
Water Required to Mix10-12%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sharadaa Ceramics Calcium Silicate Block
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables
Thermal Ceramics K-Shield Felt AG/Min-K Composite
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact

CSHARA004 / 130167

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.