MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phosphor bronze 1.25% Sn, UNS C50500, OSO35 Temper, 0.035 mm Grain Size
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability. Fabricated by blanking, bending, heading, and upsetting, shearing and swaging.

Applications: electrical contacts, flexible hose, pole-line hardware.

Test specimen: flat products - 1mm thickness.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 276 MPa40000 psi
Tensile Strength, Yield 76.0 MPa
@Strain 0.2 %
11000 psi
@Strain 0.2 %
Elongation at Break 47 %47 %In 50 mm
Modulus of Elasticity 117 GPa17000 ksi
Poissons Ratio 0.330.33
Fatigue Strength 114 MPa
@# of Cycles 1.00e+8
16500 psi
@# of Cycles 1.00e+8
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000360 ohm-cm
@Temperature 20.0 °C
0.00000360 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 208 W/m-K
@Temperature 20.0 °C
1440 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1035 - 1075 °C1895 - 1967 °F
Solidus 1035 °C1895 °F
Liquidus 1075 °C1967 °F
Annealing Point 482 - 649 °C900 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 650 °C887 - 1200 °F
Hot-Working Temperature 800 - 875 °C1470 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 98.75 %98.75 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P <= 0.35 %<= 0.35 %
Tin, Sn 1.0 - 1.7 %1.0 - 1.7 %
Zinc, Zn <= 0.30 %<= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphor bronze 8% Sn, UNS C52100, H02 Temper rod
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO35 Temper rod
Phosphor bronze 5% Sn, UNS C51000
Phosphor bronze 1.25% Sn, UNS C50500, OSO75 Temper, 0.015 mm Grain Size
Free-cutting phosphor bronze, UNS C54400

MC50500b2 / 11488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.