MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an engineering thermoplastic. This grade exhibits high chemical resistance and barrier performance. Moreover, this grade shows a high impact resistance, both at room temperature and at lower temperatures, and good creep performance. CARILON Polymer D26FX100 can also withstand short-term exposure to elevated temperatures. CARILON Polymer D26FX100 is processable on standard extrusion equipment and may be considered for the production of tubes, industrial hoses, monofilaments, coatings for cable and wire. It is also possible to coextrude CARILON Polymer D26FX100 with other materials, typically to be employed as a barrier layer in containment applications.

Data provided by Shell Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption at Saturation 0.021 %0.021 %ASTM D570
 2.1 %2.1 %ASTM D570
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 240 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 464 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Hardness, Shore D 7575ISO 868
Tensile Strength, Ultimate 55.0 MPa7980 psiASTM D638
Tensile Strength, Yield 60.0 MPa8700 psiASTM D638
Elongation at Break >= 300 %>= 300 %ASTM D638
Elongation at Yield 25 %25 %ASTM D638
Tensile Modulus 1.60 GPa232 ksiASTM D638
Flexural Strength 55.0 MPa7980 psiat 5% strain; ASTM D790
Flexural Modulus 1.60 GPa232 ksiASTM D790
Izod Impact, Notched 2.40 J/cm4.50 ft-lb/in
 0.500 J/cm
@Temperature -40.0 °C
0.937 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D256
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Taber Abrasion, mg/1000 Cycles 12121 kg load; CS-17 Wheel; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secUL-746A rating 6 (60-120 sec)
Comparative Tracking Index >= 600 V>= 600 VUL746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 90.0 °C194 °FUL-746B Long Term Relative temperature Index; Mechanical w/o Impact
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FASTM D648
Vicat Softening Point 210 °C410 °FASTM D1525
UL RTI, Mechanical with Impact 85.0 °C
@Thickness 0.750 mm
185 °F
@Thickness 0.0295 in
UL-746B
UL RTI, Mechanical without Impact 90.0 °C
@Thickness 0.750 mm
194 °F
@Thickness 0.0295 in
UL-746B
Flammability, UL94 HBHB
Oxygen Index 21 %21 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 °C464 °FAt Die

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Greene Tweed Arlon® 1000 Polyketone
Miracll E175DL Thermoplastic Polyurethane (TPUR), Polyester Grade
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
Lubrizol LifeSciences Tecothane® TT-2072D-B20 TPU – 20% Barium Sulfate

PCAR04 / 27913

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.