MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 383 FR A Polycarbonate (PC); Carbon Fiber - Flame Retardant - RoHS Compliant
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D 792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D 570
Additive Loading 20 %20 %Primary Additive
Linear Mold Shrinkage 0.00030 - 0.0015 cm/cm
@Thickness 3.20 mm
0.00030 - 0.0015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength at Break 138 MPa20000 psiASTM D 638
Elongation at Break 1.5 - 2.5 %1.5 - 2.5 %ASTM D 638
Tensile Modulus 12.8 GPa1850 ksiASTM D 638
Flexural Strength 207 MPa30000 psiASTM D 790
Flexural Modulus 12.1 GPa1750 ksiASTM D 790
Izod Impact, Notched 0.961 J/cm
@Thickness 3.20 mm
1.80 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10000 ohm-cm<= 10000 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 82.2 - 121 °C180 - 250 °F
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
Covestro Bayblend® FR3010 IF PC/ABS Blend
RTP Company RTP 305 TFE 15 SE A Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 HB
Avient Edgetek® PC-10CF/000 Polycarbonate (PC), Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced

PQZRA36301 / 205971

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.