MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, communications (bobbin, relay bed, optical cable closure), military, sports equipment (skis, helmets, foot wear), and medical equipment. Product is customizable.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Filler Content 50 %50 %Glass Fiber
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 135 MPa19600 psiASTM D638
Elongation at Break 2.3 %2.3 %ASTM D638
Flexural Strength 185 MPa26800 psiASTM D790
Flexural Modulus 8.90 GPa1290 ksiASTM D790
Izod Impact Resistance 3.20 J/cm²15.2 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 162 °C324 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 216 - 232 °C421 - 450 °F
Middle Barrel Temperature 210 - 227 °C410 - 441 °F
Front Barrel Temperature 204 - 221 °C399 - 430 °F
Melt Temperature 210 - 249 °C410 - 480 °F
Mold Temperature 38.0 - 77.0 °C100 - 171 °F
Injection Velocity 13.0 - 25.0 mm/sec0.512 - 0.984 in/sec
Injection Pressure 69.0 - 103 MPa10000 - 14900 psi
Hold Pressure 34.0 - 69.0 MPa4930 - 10000 psi
Back Pressure 0.170 - 0.340 MPa24.7 - 49.3 psi
Screw Speed 30 - 70 rpm30 - 70 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® L6 GF/40 30% Glass Fiber Reinforced Polypropylene
Techmer ES HiFill® PP GF40 CC 40% Glass Filled
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant
Hexcel® HexForce™ SA083 Fiber Glass Fabric

PZHEJ002 / 92817

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.