MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NRI Titan® 118 Carbon Fiber Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Description: The Titan®-118 structural repair system is comprised of a unique, uni-directional carbon fiber fabric, saturated with Titan®-Saturant Epoxy, and Titan®-Primer Epoxy primer system.

Typical Applications:

  • Structural strengthening of concrete or masonry structures for:
  • An increase in load requirements due to code change or design error
  • Containment and shear reinforcement
  • Seismic retrofitting
  • Structural damage
Benefits:
  • System meets all ACI 440.8-13 material specification requirements
  • ICC-ES ESR listed product
  • 100% solvent-free
  • Zero VOC system
  • Long working time, even in hot environments
  • Durable, highly resistant to aggressive environments
  • Applicable at up to 90% humidity
  • High strength and light weight

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³Dry Fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 65.5 MPa9500 psiTitan-Primer & Titan-Saturant Epoxy
 1385 MPa200900 psiComposite Gross Laminate; ASTM D3039
 3790 MPa550000 psiDry Fiber Material
Elongation at Break 1.3 %1.3 %Composite Gross Laminate; ASTM D3039
 1.5 %1.5 %Dry Fiber Material
 4.0 %4.0 %Titan-Primer & Titan-Saturant Epoxy
Tensile Modulus 2.62 GPa380 ksiTitan-Primer & Titan-Saturant Epoxy
 101.14 GPa14669 ksiComposite Gross Laminate; ASTM D3039
 230 GPa33400 ksiDry Fiber Material
Flexural Strength 100.2 MPa14530 psiTitan-Primer & Titan-Saturant Epoxy
Flexural Modulus 5.96 GPa865 ksiTitan-Primer & Titan-Saturant Epoxy
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 138 °C280 °F
Minimum Service Temperature, Air 10.0 °C50.0 °F
Glass Transition Temp, Tg 85.0 °C185 °FTitan-Primer & Titan-Saturant Epoxy
 
Processing PropertiesMetricEnglishComments
Cure Time  180 min
@Temperature 32.0 °C
3.00 hour
@Temperature 89.6 °F
Set Time
 360 min
@Temperature 24.0 °C
6.00 hour
@Temperature 75.2 °F
Set Time
 720 min
@Temperature 16.0 °C
12.0 hour
@Temperature 60.8 °F
Set Time
 1440 min
@Temperature 10.0 °C
24.0 hour
@Temperature 50.0 °F
Set Time
Pot Life 75.0 min75.0 min
Working Life  35.0 min
@Temperature 32.0 °C
35.0 min
@Temperature 89.6 °F
 75.0 min
@Temperature 24.0 °C
75.0 min
@Temperature 75.2 °F
 150 min
@Temperature 16.0 °C
150 min
@Temperature 60.8 °F
 225 min
@Temperature 10.0 °C
225 min
@Temperature 50.0 °F
Shelf Life 12.0 Month12.0 MonthEpoxy
 12.0 Month12.0 MonthFabric

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy/Carbon Fiber Composite
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Hexcel® HexTow® AS4D Carbon Fiber - Epoxy Composite
NRI Titan® 218 Carbon Fiber Composite
NRI Trans-Wrap Carbon Fiber Epoxy Composite

PNRI026 / 192042

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.