MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

304 Stainless Steel (UNS S30400); Annealed Bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Tensile property data reported is typical longitudinal.

Austenitic Cr-Ni stainless steel. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion.

Applications: beer kegs, bellows, chemical equipment, coal hopper linings, cooking equipment, cooling coils, cryogenic vessels, dairy equipment, evaporators, flatware utensils, feedwater tubing, flexible metal hose, food processing equipment, hospital surgical equipment, hypodermic needles, kitchen sinks, marine equipment and fasteners, nuclear vessels, oil well filter screens, refrigeration equipment, paper industry, pots and pans, pressure vessels, sanitary fittings, valves, shipping drums, spinning, still tubes, textile dyeing equipment, tubing.

Corrosion Resistance: resists most oxidizing acids and salt spray.

UNS S30400; AMS 5501, 5513, 5560, 5565; ASME SA182, SA194 (8), SA213, SA240; ASTM A167, A182, A193, A194

Key Words: aisi304, AISI 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, UNS S30400, AMS 5501, AMS 5513, AMS 5560, AMS 5565, AMS 5566, AMS 5567, AMS 5639, AMS 5697, ASME SA182, ASME SA194 (8), ASME SA213, ASME SA240, ASME SA249, ASME SA312, ASME SA320 (B8), ASME SA358, ASME SA376, ASME SA403, ASME SA409, ASME SA430, ASME SA479, ASME SA688, ASTM A167, ASTM A182, ASTM A193, ASTM A194, ASTM A666, FED QQ-S-763, MILSPEC MIL-S-5059, SAE 30304, DIN 1.4301, X5CrNi189, B.S. 304 S 15, EN 58E, PN 86020 (Poland), OH18N9, ISO 4954 X5CrNi189E, ISO 683/13 11, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  640 MPa
@Temperature 24.0 °C
92800 psi
@Temperature 75.2 °F
 640 MPa
@Temperature 24.0 °C
92800 psi
@Temperature 75.2 °F
 1150 MPa
@Temperature -78.0 °C
167000 psi
@Temperature -108 °F
 1150 MPa
@Temperature -78.0 °C
167000 psi
@Temperature -108 °F
 1520 MPa
@Temperature -196 °C
220000 psi
@Temperature -321 °F
 1520 MPa
@Temperature -196 °C
220000 psi
@Temperature -321 °F
 1720 MPa
@Temperature -269 °C
249000 psi
@Temperature -452 °F
 1720 MPa
@Temperature -269 °C
249000 psi
@Temperature -452 °F
 1860 MPa
@Temperature -253 °C
270000 psi
@Temperature -423 °F
 1860 MPa
@Temperature -253 °C
270000 psi
@Temperature -423 °F
Tensile Strength, Yield  235 MPa
@Temperature 24.0 °C
34100 psi
@Temperature 75.2 °F
 235 MPa
@Temperature 24.0 °C
34100 psi
@Temperature 75.2 °F
 280 MPa
@Temperature -196 °C
40600 psi
@Temperature -321 °F
 280 MPa
@Temperature -196 °C
40600 psi
@Temperature -321 °F
 300 MPa
@Temperature -78.0 °C
43500 psi
@Temperature -108 °F
 300 MPa
@Temperature -78.0 °C
43500 psi
@Temperature -108 °F
 400 MPa
@Temperature -269 °C
58000 psi
@Temperature -452 °F
 400 MPa
@Temperature -269 °C
58000 psi
@Temperature -452 °F
 420 MPa
@Temperature -253 °C
60900 psi
@Temperature -423 °F
 420 MPa
@Temperature -253 °C
60900 psi
@Temperature -423 °F
Elongation at Break  27 %
@Temperature -253 °C
27 %
@Temperature -423 °F
 27 %
@Temperature -253 °C
27 %
@Temperature -423 °F
 30 %
@Temperature -269 °C
30 %
@Temperature -452 °F
 30 %
@Temperature -269 °C
30 %
@Temperature -452 °F
 45 %
@Temperature -196 °C
45 %
@Temperature -321 °F
 45 %
@Temperature -196 °C
45 %
@Temperature -321 °F
 50 %
@Temperature -78.0 °C
50 %
@Temperature -108 °F
 50 %
@Temperature -78.0 °C
50 %
@Temperature -108 °F
 76 %
@Temperature 24.0 °C
76 %
@Temperature 75.2 °F
 76 %
@Temperature 24.0 °C
76 %
@Temperature 75.2 °F
Reduction of Area  54 %
@Temperature -253 °C
54 %
@Temperature -423 °F
 54 %
@Temperature -253 °C
54 %
@Temperature -423 °F
 55 %
@Temperature -269 °C
55 %
@Temperature -452 °F
 55 %
@Temperature -269 °C
55 %
@Temperature -452 °F
 66 %
@Temperature -196 °C
66 %
@Temperature -321 °F
 66 %
@Temperature -196 °C
66 %
@Temperature -321 °F
 76 %
@Temperature -78.0 °C
76 %
@Temperature -108 °F
 76 %
@Temperature -78.0 °C
76 %
@Temperature -108 °F
 82 %
@Temperature 24.0 °C
82 %
@Temperature 75.2 °F
 82 %
@Temperature 24.0 °C
82 %
@Temperature 75.2 °F
Modulus of Elasticity 193 GPa28000 ksi
Notched Tensile Strength  710 MPa
@Temperature 24.0 °C
103000 psi
@Temperature 75.2 °F
 710 MPa
@Temperature 24.0 °C
103000 psi
@Temperature 75.2 °F
 1060 MPa
@Temperature -196 °C
154000 psi
@Temperature -321 °F
 1060 MPa
@Temperature -196 °C
154000 psi
@Temperature -321 °F
 1120 MPa
@Temperature -253 °C
162000 psi
@Temperature -423 °F
 1120 MPa
@Temperature -253 °C
162000 psi
@Temperature -423 °F
Poissons Ratio 0.290.29
Shear Modulus 77.0 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000720 ohm-cm
@Temperature 20.0 °C
0.0000720 ohm-cm
@Temperature 68.0 °F
 0.000116 ohm-cm
@Temperature 650 °C
0.000116 ohm-cm
@Temperature 1200 °F
Magnetic Permeability 1.0201.020at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
9.89 µin/in-°F
@Temperature 32.0 - 599 °F
 18.4 µm/m-°C
@Temperature 0.000 - 538 °C
10.2 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.2 W/m-K
@Temperature 0.000 - 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 32.0 - 212 °F
 21.5 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 66.345 - 74 %66.345 - 74 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 10.5 %8.0 - 10.5 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed bar
304 Stainless Steel
303 Stainless Steel, annealed bar
Titanium Ti-6Al-4V (Grade 5), Annealed
304 Stainless Steel (UNS S30400); Cold Finished and Annealed Bar

MQ304A18 / 151040

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.