MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow

Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin with improved flow. It is also a PPA

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inDAM; ISO 294-4 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psi50%RH; ISO 527-1/-2
 145 MPa21000 psiDAM; ISO 527-1/-2
Elongation at Break 1.9 %1.9 %50%RH; ISO 527-1/-2
 2.1 %2.1 %DAM; ISO 527-1/-2
Tensile Modulus 10.7 GPa1550 ksiDAM; ISO 527-1/-2
 11.3 GPa1640 ksi50%RH; ISO 527-1/-2
Flexural Strength 200 MPa29000 psi50%RH; ISO 178
 225 MPa32600 psiDAM; ISO 178
Flexural Modulus 9.80 GPa1420 ksiDAM; ISO 178
 10.8 GPa1570 ksi50%RH; ISO 178
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²50%RH; ISO 179/1eU
 4.50 J/cm²21.4 ft-lb/in²DAM; ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²DAM; ISO 179/1eA
 0.700 J/cm²3.33 ft-lb/in²50%RH; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FDAM; ISO 11359-1/-2
 12.0 µm/m-°C
@Temperature 55.0 - 160 °C
6.67 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
 18.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
10.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 62.0 µm/m-°C34.4 µin/in-°FDAM; ISO 11359-1/-2
 60.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 95.0 µm/m-°C
@Temperature 55.0 - 160 °C
52.8 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Melting Point 310 °C590 °FDAM; first heat; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 281 °C538 °FDAM; ISO 75-1/-2
UL RTI, Electrical  140 °C
@Thickness 0.400 mm
284 °F
@Thickness 0.0157 in
UL 746B
 140 °C
@Thickness 0.800 mm
284 °F
@Thickness 0.0315 in
DAM; UL 746B
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
DAM; UL 746B
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
DAM; IEC 60695-11-10
 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
DAM; IEC 60695-11-10
Oxygen Index 37 %37 %DAM; ISO 4589-1/-2
Glow Wire Test  700 °C
@Thickness 0.400 mm
1290 °F
@Thickness 0.0157 in
DAM; IEC 60695-2-1/2
 775 °C
@Thickness 3.00 mm
1430 °F
@Thickness 0.118 in
DAM; IEC 60695-2-1/3
 960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
DAM; IEC 60695-2-1/2
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
DAM; IEC 60695-2-1/2
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PA6T/66-GF30FR<ISO 11469
 >PPA-GF30FR<SAE J1344
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
UL recognitionULDAM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Celanese Zytel® HTN 51G50HSL BK083 Polyphthalamide (PPA)

PZDSY5459 / 161286

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.