MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE
Categories: Polymer; Adhesive

Material Notes: 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated with oil typically used with machine parts.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.7 microns0.500 milCarrier
 43.2 microns1.70 milFaceside Adhesive
 43.2 microns1.70 milBackside Adhesive
 99.1 microns3.90 milTotal Thickness
 107 microns4.20 milCaliper
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.877 kN/m5.00 pliABS, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 0.93128 kN/m5.3125 pliStainless Steel, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 1.0408 kN/m5.9375 pliPP, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 1.205 kN/m6.875 pliPC, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 1.205 kN/m6.875 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 1.205 kN/m6.875 pliABS, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 1.205 kN/m6.875 pliPP, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 1.53 kN/m8.75 pliPC, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 55.1 kV/mm1400 kV/in
Dielectric Breakdown 5600 V5600 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FLong term
 149 °C300 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type300LSE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M ATG 924 Tape
3M 9731 Double Coated Tape
3M F-9465PC Adhesive Transfer Tape
3M 6969 Duct Tape
Solvay Flashtape 1R Adhesive tape

PMM33272 / 168019

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.