MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 V PEI
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Semitron™ ESd 420V PEI electrostatic dissipative shapes possess high strength and stiffness and are not subject to dimensional change when exposed to moisture.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Water Absorption at Saturation 1.40 %1.40 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 112112ASTM D785
Tensile Strength 70.0 MPa10200 psiISO 527-1/-2 (7)
Compressive Yield Strength  44.0 MPa
@Strain 1.00 %
6380 psi
@Strain 1.00 %
ISO 604 (10)
 89.0 MPa
@Strain 2.00 %
12900 psi
@Strain 2.00 %
ISO 604 (10)
 169 MPa
@Strain 5.00 %
24500 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+6 ohm1.00e+6 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C15.0 µin/in-°FASTM E-831 (TMA)
 30.0 µm/m-°C
@Temperature 23.0 - 100 °C
16.7 µin/in-°F
@Temperature 73.4 - 212 °F
 30.0 µm/m-°C
@Temperature 23.0 - 150 °C
16.7 µin/in-°F
@Temperature 73.4 - 302 °F
 34.0 µm/m-°C
@Temperature >=150 °C
18.9 µin/in-°F
@Temperature >=302 °F
Maximum Service Temperature, Air 171 °C340 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 216 °C420 °FASTM D648
Glass Transition Temp, Tg 216 °C420 °FDMA- Tan d
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic LimitedLimited
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 PEI Static Dissipative Polyetherimide
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Mitsubishi Chemical Advanced Materials Semitron™ MDS 100 PEEK
Mitsubishi Chemical Advanced Materials Semitron™ CMP LL5 PET Polyester
Mitsubishi Chemical Advanced Materials Semitron™ CMP XL20 PAI

P1SM32B / 20122

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.