MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm Acrylite® SG Acrylic Sheet, Sign Grade
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified Sheet

Material Notes: Data provided by CYRO Industries

Continuously manufactured sheet developed for the sign market. Versatile, tough, lightweight, easy to fabricate and machine. Cutting, routing, drilling, forming, and cementing can be performed on this product. Used for channel letters, formed letters, and shapes a well as back-painted signs.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %24 hrs, 23°C; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8282ASTM D785
Tensile Strength, Ultimate 61.0 MPa8850 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 2.60 GPa377 ksiASTM D638
Flexural Yield Strength 97.0 MPa14100 psiASTM D790
Flexural Modulus 2.74 GPa397 ksiASTM D790
Izod Impact, Notched 0.340 J/cm0.637 ft-lb/inASTM D256
Gardner Impact 2.30 J1.70 ft-lbB; ASTM D3029
Instrumented Impact Total Energy 6.20 J4.57 ft-lbInstrumented dart, total energy; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 20.0 °C
40.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.47 J/g-°C0.351 BTU/lb-°Ftypical of Acrylite® sheet
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°Ftypical of Acrylite® sheet
Maximum Service Temperature, Air 71.0 °C160 °F
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °FASTM D648
Vicat Softening Point 106 °C223 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Gloss 125 %125 %20°; ASTM D523
Transmission, Visible 90 %90 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 165 °C275 - 329 °Fforming temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® SG10 Acrylic
Spartech Polycast Cell Cast Acrylic
Aluminum 5052-H32
Röhm Acrylite® 8N Acrylic Polymer
Lucite International SW Sanitary Ware Acrylic Sheet

PCYR31 / 29170

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.