Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fatigue strength and toughness is required. The material is resistant to boiling water, a broad range of chemicals and to stress cracking. Articles can be easily produced by injection molding or extrusion. Grilamid XE 4010 offers a variety of interesting properties such as:- High transparency
- High gloss
- High fatigue strength
- Resistance to boiling water
- Resistance to a broad range of solvents and chemicals
- Excellent toughness
- Low density
- Outstanding weather resistance