MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shanghai Ofluorine J-2 PVDF Extrusion Grade
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Description: J-2 PVDF is a kind of granules homopolymer, which has middle melt viscosity, J-2 is more suitable for extrusion process. J-2 PVDF pellets as raw materials, the finished products has excellent mechanical strength and flexibility. It can not be eroded by acid, alkali, strong oxidant, halogens. Good durability to aliphatic hydrocarbons, aromatic hydrocarbons, alcohol, aldehyde etc. In the work of hydrochloric acid, nitric acid, sulfuric acid, dilute alkali liquor, dense alkali liquor(40%) and 100°C, which keep stable. Others, J-2 PVDF finished products has the properties of ?-Ray resistant, UV resistant, and stability in wide temperature range.

Application: manufacture PVDF tubes, PVDF pipes, PVDF valves etc.

Information provided by Shanghai Ofluorine Chemical Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.77 - 1.79 g/cc1.77 - 1.79 g/ccASTM D792
Water Absorption <= 0.050 %<= 0.050 %ASTM D570
Melt Flow 5.0 - 10 g/10 min
@Load 10.0 kg,
Temperature 230 °C
5.0 - 10 g/10 min
@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 8070 - 80ASTM D2240
Tensile Strength at Break >= 30.0 MPa>= 4350 psi50mm/min; ASTM D638
Tensile Strength, Yield >= 40.0 MPa>= 5800 psi50mm/min; ASTM D638
Elongation at Break >= 50 %>= 50 %50mm/min; ASTM D638
Elongation at Yield 5.0 - 10 %5.0 - 10 %50mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 171 °C329 - 340 °F10°C/min; ASTM D3418
Flammability, UL94 V-0V-0
 
Descriptive Properties
AppearanceWhite translucent pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zotefoams ZOTEK® F 30 PVDF Foam
Teknor Apex Elexar® EL 1934E Thermoplastic Elastomer
Shanghai Ofluorine 9201 PVDF Pellets for cables
ScanTube ETFE Tubing
Omnia Plastica Kynar® PVDF

PSHANGO05 / 130336

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.