MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Nylon 6.6 for injection molding, maximum cold and dry impact resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Water Absorption 1.1 - 1.9 %1.1 - 1.9 %ISO 62
Water Absorption at Saturation 6.0 - 8.0 %6.0 - 8.0 %ISO 62
Viscosity Measurement 145145Viscosity index; ISO 307
Linear Mold Shrinkage 0.015 - 0.025 cm/cm0.015 - 0.025 in/inFRISETTA Test Method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 95.0 MPa13800 psiISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psiISO 527
Elongation at Break 63 %63 %ISO 527
Tensile Modulus 1.80 GPa261 ksiISO 527
Flexural Strength 55.0 MPa7980 psiISO 178
Charpy Impact, Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DIN 53453
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact Unnotched NBNBISO 179/1eU
 NBNBDIN 53453
Charpy Impact, Notched 4.40 J/cm²20.9 ft-lb/in²DIN 53453
 NBNBISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 V600 VCTI 100; IEC 112
 600 V600 VCTI-M 100; IEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 3146 DSC
Maximum Service Temperature, Air 90.0 °C194 °FContinuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 440 TPC, Unfilled
Celanese Vandar® 2100UV PBT, Impact Modified
Celanese Vandar® 2100 PBT, Unfilled
Celanese Riteflex® 655HS TPC, Unfilled
Celanese Riteflex® 640 Thermoplastic Polyester Elastomer (TPE)

PFRI043 / 38964

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.