MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schunk FE45A Electrographite Antimony Impregnated
Categories: Carbon; Graphite

Material Notes: Typical Application Fields: Carbon bearings and mechanical seals applied at high temperatures.

Information provided by Schunk Graphite Technology, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.50 g/cc0.0903 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 75755/62.5
Hardness, Rockwell B 1151155/100
Modulus of Elasticity 16.0 GPa2320 ksi
Flexural Strength 65.0 MPa9430 psi
Compressive Strength 170 MPa24700 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.50 µm/m-°C
@Temperature 20.0 - 200 °C
2.50 µin/in-°F
@Temperature 68.0 - 392 °F
 5.00 µm/m-°C
@Temperature 200 - 600 °C
2.78 µin/in-°F
@Temperature 392 - 1110 °F
Thermal Conductivity 67.0 W/m-K465 BTU-in/hr-ft²-°F
 
Descriptive Properties
Inert Atmosphere600°C
Oxidizing Atmosphere500°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PSM Industries Pacific Sintered Metals SS-410-R 410 Stainless Steel Powdered Metal (MPIF SS-410-95)
Schunk FH82A Carbon Graphite Antimony Impregnated
410 Stainless Steel
CoorsTek CRB-300 General-Duty Carbon Graphite
CoorsTek CRB-400 Antimony-Impregnated Carbon Graphite

CSCHU023 / 194780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.