MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grilamid® L 20 G HL PA12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description: Grilamid L 20 GHL is a, medium viscosity injection molding grade, based on Polyamide 12 (PA12). Grilamid L 20 GHL is UV-stabilized, and heat stabilized The special features of Grilamid L 20 GHL are:
  • Good UV-resistance:
    • Improved heat stability
    • Good resistance to chemicals and oils
    • High surface finish quality
    • Low abrasion
    • Good dimensional stability
    • Low density, low weight
    Application examples: Grilamid L 20 GHL is suitable for high precision applications in automotive, electrical, and industrial market sectors where high heat and UV resistance are required.

    Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %ISO 62
Moisture Absorption 0.700 %0.700 %ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 70.0 MPa10200 psiconditioned; ISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psiconditioned; ISO 527-1/-2
 60.0 MPa8700 psidry; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa5800 psiconditioned; ISO 527-1/-2
 50.0 MPa7250 psidry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %conditioned; ISO 527-1/-2
 <= 50 %<= 50 %dry; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %dry; ISO 527-1/-2
 12 %12 %conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa160 ksiconditioned; ISO 527-1/-2
 1.60 GPa232 ksidry; ISO 527-1/-2
Charpy Impact Unnotched NBNBdry; ISO 179/1eU
 NBNBconditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²dry; ISO 179/1eA
 0.700 J/cm²3.33 ft-lb/in²conditioned; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inconditioned; IEC 60243-1
Comparative Tracking Index 550 V550 Vconditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C194 - 230 °Flong term; EMS
 150 °C302 °Fshort term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical equipment
 Energy distribution
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Tools & Accessories
ProcessingInjection Molding
Product AttributesNucleated
Special CharacteristicsImproved heat resistance
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 55 LX PA12/MACMI
EMS-Grivory Grilamid® L 20 W 20 PA12
EMS-Grivory Grilamid® L 20 LF grey PA12
EMS-Grivory Grilamid® L 20 HL black 9563 PA12
EMS-Grivory Grilamid® L 20 G PA12

PGRH026 / 156735

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.