MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hybrid S464G20 PC/ABS, 20% Glass Filled, DAM
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled

Material Notes:

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527-1
Elongation at Break 3.0 %3.0 %ISO 527-1
Flexural Strength 121 MPa17500 psiISO 178
Flexural Modulus 5.40 GPa783 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FISO 75-2A
Shrinkage, MD 0.10 - 0.30 %
@Thickness 3.17 mm
0.10 - 0.30 %
@Thickness 0.125 in
ISO 294-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daicel CEVIAN® S5220 20% GF PC/ABS alloy
Daicel CEVIAN® S1220 PC/ABS alloy
Daicel CEVIAN® S5210 10% GF PC/ABS alloy
Polykemi AB POLYblend 45FS GF20 PC/ABS-Blend, Glass Fiber reinforced
Lotte Advanced Materials Infino® WP-1200 PC/ABS/GF

PRAVAGO1397 / 221929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.