MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unitika TERRAMAC TP-4000 Polylactic Acid (PLA)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Basic grade, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Melt Flow 3.0 - 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 - 5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 66.0 MPa9570 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Flexural Strength 108 MPa15700 psiISO 178
Flexural Modulus 4.60 GPa667 ksiISO 178
Charpy Impact, Notched 0.160 J/cm²0.761 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 °C338 °F
Maximum Service Temperature, Air 240 °C464 °F
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C138 °FISO 75
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 150 - 180 °C302 - 356 °F
Middle Barrel Temperature 160 - 200 °C320 - 392 °F
Front Barrel Temperature 160 - 200 °C320 - 392 °F
Nozzle Temperature 150 - 180 °C302 - 356 °F
 
Descriptive Properties
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unitika TERRAMAC TP-4030 Polylactic Acid (PLA)
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA)
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA)
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA)

PUNITIK907 / 177927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.