MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® Vasco® 450 Specialty Steel, Heat Treatment: 1038°C (1900°F) + Age  (discontinued **)
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Data provided by Allvac.

Applications: Land-based turbine blades and buckets.

Key Words: Allvac, an Allegheny Teledyne Company, UNS S45000; AMS 5763, 5773. ASTM A 564/564 M, A 705/705 M
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 318318Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 346346Estimated from Rockwell C value.
Hardness, Rockwell C 3434
Hardness, Vickers 333333Estimated from Rockwell C value.
Tensile Strength, Ultimate 1035 MPa150100 psi
Tensile Strength, Yield 966 MPa
@Strain 0.2 %
140000 psi
@Strain 0.2 %
Elongation at Break 18 %18 %
Reduction of Area 65 %65 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.025 %0.025 %
Chromium, Cr 15 %15 %
Copper, Cu 1.5 %1.5 %
Iron, Fe 76 %76 %as balance
Manganese, Mn 0.50 %0.50 %
Molybdenum, Mo 0.75 %0.75 %
Nickel, Ni 6.0 %6.0 %
Phosphorus, P 0.015 %0.015 %
Silicon, Si 0.50 %0.50 %
Sulfur, S 0.015 %0.015 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
440C Martensitic Stainless Steel (UNS S44004)
AISI Type 440B Stainless Steel
440A Martensitic Stainless Steel (UNS S44002)
AK Steel 420 Martensitic Stainless steel
Crucible Steel 440B Chromium Steel

NALL87 / 14819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.