MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Breplast Bretene TS COR Plus T15 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Recovered polyethylene composite

Information provided by Breplast S.p.A.

Key Words: Extrusion
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.950 g/cc>= 0.0343 lb/in³UNI EN ISO 1183-1
Melt Flow  0.20 - 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 - 0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
UNI EN ISO 1133
 1.0 - 1.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.0 - 1.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
UNI EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 16.0 MPa2320 psiISO 527-1-2
Elongation at Break 550 %550 %ISO 527
 
Descriptive Properties
ColorGrey / Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Breplast Bretene TS COR Plus T10 High Density Polyethylene
Breplast Bretene HD Bottles Thin Flakes High Density Polyethylene
Breplast Bretene TS COR Plus High Density Polyethylene
Braskem UTEC® 6541 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene

PBREP912 / 159357

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.