MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay ALBRITECT® CP 40 Vinyl phosphonic acid - acrylic acid copolymer, 40% aqueous Solution
Categories: Fluid; Polymer

Material Notes: Vinyl phosphonic acid - acrylic acid copolymer

Identification: VINYL PHOSPHONIC ACID – ACRYLIC ACID COPOLYMER (40% SOLUTION WATER)

CAS: 27936 – 88 – 5

Solubility in water: Miscible (in all proportions)

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Pretreatment of aluminum and zinc. Replacement of chromic acid in conversion treatments.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Solids Content 36 - 44 %36 - 44 %AM6275
pH 1.01.0Aqueous solution-1%
Molecular Weight 30000 - 90000 g/mol30000 - 90000 g/molAM6273
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceYellow to brown liquid
CompositionResidual acrylic acid<1.0%, AM6272
 Residual vinyl phosphonic acid<2.0%, AM6272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ALBRITECT® CP 30 Vinyl phosphonic acid - acrylic acid copolymer, 20% Aqueous solution

WRHOD015 / 137245

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.