MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silver-bearing tough pitch Copper, UNS C11400, M20 Temper flat products, rod, shapes
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: gaskets, radiators, busbars, windings, switches, chemical process equipment, clad metals, printed circuit foil.

Test specimens: flat products - 6mm thickness, rod - 25mm diameter, and shapes - 13mm diameter.

Key Words: CDA 114 STP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 - 8.94 g/cc0.321 - 0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 4040
Tensile Strength, Ultimate 220 MPa31900 psi
Tensile Strength, Yield 69.0 MPa10000 psi
Elongation at Break 55 %55 %in 50 mm, rod
 50 %
@Thickness 6.00 mm
50 %
@Thickness 0.236 in
in 50 mm, shapes
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %UNS C37700 (forging brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 150 MPa21800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000172 ohm-cm
@Temperature 20.0 °C
0.00000172 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 388 W/m-K
@Temperature 20.0 °C
2690 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1080 °C<= 1980 °F
Liquidus 1080 °C1980 °F
Annealing Point 482 - 760 °C900 - 1400 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 750 °C887 - 1380 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99 - 99.9 %99 - 99.9 %
Oxygen, O <= 0.040 %<= 0.040 %
Silver, Ag <= 0.034 %<= 0.034 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free silver-bearing Copper, UNS C10400, H04 Temper wire
Avient Edgetek® NJ-30GF/000 Nylon 12, Glass Filled
Silver-bearing tough pitch Copper, UNS C11400, OSO50 Temper wire
Silver-bearing tough pitch Copper, UNS C11400, M30 Temper shapes
Silver-bearing tough pitch Copper, UNS C11400, H08 Temper wire

MC11400c5 / 10562

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.