MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sylvania SD151 Molybdenum Thermal Spray Powder
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: General Description

SD151 is a premium grade molybdenum powder. Particles are fully dense and free flowing, allowing for higher spray rates - up to twice the spray rate of comparable SA-type powders.

Applications

  • Any application which requires high flow rates and high apparent densities
  • Components in aircraft turbines

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 5.00 g/cc0.181 lb/in³
Particle Mesh Size 170 Mesh170 Mesh1% bigger
 200 Mesh200 Mesh15% bigger
 325 Mesh325 Mesh80% bigger
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo >= 99.5 %>= 99.5 %
O2 <= 0.15 %<= 0.15 %
 
Descriptive Properties
Hall Flow, seconds/50g8-15ASTM B213

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Molybdenum Disilicide, MoSi2
Sylvania SA101 Molybdenum Thermal Spray Powder
Sylvania SD152 Molybdenum Thermal Spray Powder
Sylvania SA901A/B Molybdenum Thermal Spray Powder
Platinum-5 Molybdenum Thermocouple Alloy

CSYLV01 / 2300

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.