BASF Ultraform® N2650 Z4 POM + PUR
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, Unreinforced
Material Notes:
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.850
g/cc
0.0307
lb/in³
Density
1.35
g/cc
0.0488
lb/in³
ISO 1183
Water Absorption
0.80 %
0.80 %
ISO 62
Moisture Absorption at Equilibrium
0.20 %
0.20 %
ISO 62
Melt Flow
9.45
g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.45
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
45.0
MPa
6530
psi
50 mm/min; ISO 527-1/-2
Elongation at Break
40 %
40 %
50 mm/min, Nominal; ISO 527-1/-2
Elongation at Yield
16 %
16 %
50 mm/min; ISO 527-1/-2
Tensile Modulus
1.50
GPa
218
ksi
ISO 527-1/-2
Charpy Impact Unnotched
27.0
J/cm²
@Temperature -30.0 °C
128
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.800
J/cm²
@Temperature -30.0 °C
3.81
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
1.50
J/cm²
@Temperature 23.0 °C
7.14
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours
950
MPa
@Strain <=0.5 %
138000
psi
@Strain <=0.5 %
ISO 899-1
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
IEC 60093
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
IEC 60093
Dielectric Constant
4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor
0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
600
V
Test Solution A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
130
µm/m-°C
@Temperature 23.0 - 55.0 °C
72.2
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point
167
°C
333
°F
ISO 11357-1/-3
Maximum Service Temperature, Air
100
°C
212
°F
Deflection Temperature at 1.8 MPa (264 psi)
80.0
°C
176
°F
ISO 75-1/-2
Decomposition Temperature
>=
240
°C
>=
464
°F
Ignition Temperature
320
-
340
°C
608
-
644
°F
ASTM D1929
Processing Properties
Metric
English
Comments
Processing Temperature
200
°C
392
°F
Hopper Throat
Zone 1
200
°C
392
°F
Feed zone
Zone 2
200
°C
392
°F
Compression
Zone 3
200
°C
392
°F
Metering-zone
Zone 4
200
°C
392
°F
Nozzle
Melt Temperature
200
°C
392
°F
Optimal
190
-
215
°C
374
-
419
°F
Injection molding
Mold Temperature
60.0
°C
140
°F
Optimal
60.0
-
80.0
°C
140
-
176
°F
Injection molding
Drying Temperature
100
°C
212
°F
Dry Time
3
hour
3
hour
Descriptive Properties
Commercial Status
Europe
Peripheral Screw Speed
<0.3 m/s
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultraform® N2640 Z2 POM + PUR
BASF Ultraform® N2644 Z9 POM + PUR
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer
PBASG0165 / 131798
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.