MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 6 IMP NC Q1A501 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Unreinforced and modified polyamide 6, with improved good-impact resistance, heat stabilized, lubricated for injection molding. Eplamid 6 IMP A501 is used in all sectors of industry, offering a good impact resistance.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Linear Mold Shrinkage 0.014 cm/cm0.014 in/inParallel; ISO 294-4
 0.020 cm/cm0.020 in/inNormal; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 35.0 MPa5080 psiConditioned; ISO 527-2
 60.0 MPa8700 psiDry; ISO 527-2
Elongation at Break >= 30 %>= 30 %Conditioned; ISO 527-2
 >= 40 %>= 40 %Dry; ISO 527-2
Tensile Modulus 1.20 GPa174 ksiConditioned; ISO 527-2
 2.40 GPa348 ksiDry; ISO 527-2
Flexural Strength 85.0 MPa12300 psiISO 178
Flexural Modulus 2.05 GPa297 ksiISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-2/A
Vicat Softening Point 190 °C374 °FISO 306/B50
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
EN 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epsan Eplamid 66 IMP NC Q1A501 Polyamide 66

PEPSAN066 / 186380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.