MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxford Polymers PEEK 450-INJ-Black PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Product Description: Polyetheretherketone, general purpose injection molding grade

Processing and Delivery Form: Pellets and Injection Molding

Additives: Carbon black

Special Characteristics: Precolored black

Information provided by Oxford Polymers

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
Water Absorption at Saturation 0.10 %0.10 %ASTM D570
Linear Mold Shrinkage, Flow 0.011 cm/cm
@Thickness 3.17 mm
0.011 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 96.5 MPa14000 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Flexural Strength 150 MPa21800 psiASTM D790
Flexural Modulus 3.59 GPa520 ksiASTM D790
Izod Impact, Notched 0.587 J/cm
@Thickness 3.17 mm
1.10 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 157 °C315 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 332 - 349 °C630 - 660 °F
Middle Barrel Temperature 349 - 366 °C660 - 690 °F
Front Barrel Temperature 354 - 371 °C670 - 700 °F
Nozzle Temperature 360 - 371 °C680 - 700 °F
Melt Temperature 354 - 377 °C670 - 710 °F
Mold Temperature 149 - 177 °C300 - 350 °F
Drying Temperature <= 149 °C<= 300 °F
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PEEK 450 BK
Aluminum 7075-O
Mitsubishi Lemalloy® BX503A-1 PPE-PA6 Alloy
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
A. Schulman Lucent PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade

POXF013 / 178443

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.